ANSI\/ASME B36.10M, B36.19m paksuse andmetabel
May 12, 2025
Jäta sõnum
ANSI\/ASME B36.10M, B36.19m paksuse andmetabel
| Nominaalne suurus (tolli) | SCH5S | SCH10S | Sch10 | Sch20 | SCH30 | SCH40S | Std | SCH40 | sch60 | SCH80S | XS | sch80 | SCH100 | SCH120 | SCH140 | SCH160 | Xxs | SCH160S |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 1/8 | 10.29 | - | 1.24 | - | - | 1.73 | 1.73 | 1.73 | 2.41 | 2.41 | 2.41 | - | - | - | - | - | - | - |
| 1/4 | 13.72 | - | 1.65 | - | - | 2.24 | 2.24 | 2.24 | 3.02 | 3.02 | 3.02 | - | - | - | - | - | - | - |
| 3/8 | 17.15 | - | 1.65 | - | - | 2.31 | 2.31 | 2.31 | 3.20 | 3.20 | 3.20 | - | - | - | - | - | - | - |
| 1/2(15) | 21.34 | 1.65 | 2.11 | - | - | 2.77 | 2.77 | 2.77 | 3.73 | 3.73 | 3.73 | - | - | - | 4.78 | 7.47 | 4.78 | - |
| 3/4(20) | 26.67 | 1.65 | 2.11 | - | - | 2.87 | 2.87 | 2.87 | 3.91 | 3.91 | 3.91 | - | - | - | 5.56 | 7.82 | 5.56 | - |
| 1(25) | 33.40 | 1.65 | 2.77 | - | - | 3.38 | 3.38 | 3.38 | 4.55 | 4.55 | 4.55 | - | - | - | 6.35 | 9.09 | 6.35 | - |
| 1 1/4(32) | 42.16 | 1.65 | 2.77 | - | - | 3.56 | 3.56 | 3.56 | 4.85 | 4.85 | 4.85 | - | - | - | - | 9.70 | - | - |
| 1 1/2(40) | 48.26 | 1.65 | 2.77 | - | - | 3.68 | 3.68 | 3.68 | 5.08 | 5.08 | 5.08 | - | - | - | - | 7.14 | 15.15 | 7.14 |
| 2(50) | 60.33 | 1.65 | 2.77 | - | - | 3.91 | 3.91 | 3.91 | 5.54 | 5.54 | 5.54 | - | - | - | - | 9.14 | 11.07 | 8.74 |
| 2 1/2(65) | 73.03 | 2.11 | 3.05 | - | - | 5.16 | 5.16 | 5.16 | 7.01 | 7.01 | 7.01 | - | - | - | - | 9.53 | 14.02 | 9.53 |
| 3(80) | 88.90 | 2.11 | 3.05 | - | - | 5.74 | 5.74 | 5.74 | 7.62 | 7.62 | 7.62 | - | - | - | - | 11.13 | 15.24 | 11.13 |
| 3 1/2(90) | 101.60 | 2.11 | 3.05 | - | - | 6.02 | 6.02 | 6.02 | 8.56 | 8.56 | 8.56 | - | - | - | 11.12 | 13.49 | 17.12 | 13.49 |
| 4(100) | 114.30 | 2.11 | 3.05 | - | - | 6.02 | 6.02 | 6.02 | 8.56 | 8.56 | 8.56 | - | - | - | 11.12 | 13.49 | 17.12 | 13.49 |
| 5(125) | 141.30 | 2.77 | 3.40 | - | - | 6.55 | 6.55 | 6.55 | 9.53 | 9.53 | 9.53 | - | - | - | 12.70 | 15.88 | 19.05 | 15.88 |
| 6(150) | 168.27 | 2.77 | 3.40 | - | - | 7.11 | 7.11 | 7.11 | 10.97 | 10.97 | 10.97 | - | - | - | 14.09 | 19.27 | 18.62 | 19.27 |
| 8(200) | 219.08 | 2.77 | 3.76 | 6.35 | 7.04 | 8.18 | 8.18 | 9.18 | 13.20 | 12.70 | 12.70 | 15.09 | 19.26 | 20.62 | 23.81 | 22.23 | 23.81 | |
| 10(250) | 273.05 | 3.40 | 4.19 | 6.35 | 7.80 | 9.27 | 9.27 | 9.27 | 12.70 | 12.70 | 12.70 | 15.09 | 19.26 | 21.44 | 25.40 | 28.58 | 25.40 | |
| 12(300) | 323.85 | 3.96 | 4.67 | 6.35 | 8.38 | 9.53 | 9.53 | 10.31 | 14.27 | 12.70 | 12.70 | 17.48 | 21.44 | 25.40 | 28.58 | 33.32 | 25.40 | |
| 14(350) | 355.60 | 3.96 | 4.78 | 6.35 | 7.92 | 9.53 | 9.53 | 11.13 | 15.09 | 12.70 | 12.70 | 19.05 | 23.81 | 27.79 | 31.75 | 35.71 | 25.40 | |
| 16(400) | 406.40 | 4.19 | 4.78 | 6.35 | 7.92 | 9.53 | 9.53 | 12.70 | 16.66 | 12.70 | 12.70 | 21.44 | 28.39 | 30.96 | 35.53 | 40.49 | 25.40 | |
| 18(450) | 457.20 | 4.19 | 4.78 | 6.35 | 7.92 | 11.13 | 9.53 | 14.27 | 19.05 | 12.70 | 12.70 | 23.81 | 29.36 | 34.33 | 38.67 | 45.24 | 25.40 | |
| 20(500) | 508.00 | 4.78 | 5.54 | 6.35 | 9.53 | 12.70 | 9.53 | 15.09 | 20.62 | 12.70 | 12.70 | 26.19 | 32.54 | 38.10 | 44.45 | 50.01 | 25.40 | |
| 22(550) | 558.80 | 4.78 | 5.54 | 6.35 | 9.53 | 12.70 | 9.53 | 22.23 | 12.70 | 12.70 | 28.58 | 34.93 | 41.26 | 47.63 | 53.98 | 25.40 | - | |
| 24(600) | 609.60 | 5.54 | 6.35 | 6.35 | 9.53 | 14.27 | 9.53 | 17.48 | 24.61 | 12.70 | 12.70 | 30.96 | 38.89 | 46.02 | 52.37 | 59.54 | - | |
| 26(650) | 660.40 | - | - | 7.92 | 12.70 | - | 9.53 | - | - | 12.70 | 12.70 | - | - | - | - | - | - | - |
| 28(700) | 711.20 | - | - | 7.92 | 12.70 | - | 9.53 | - | - | 12.70 | 12.70 | - | - | - | - | - | - | - |
| 30(750) | 762.00 | - | - | 7.92 | 12.70 | - | 9.53 | - | - | 12.70 | 12.70 | - | - | - | - | - | - | - |
| 32(800) | 812.80 | 6.35 | 7.92 | 7.92 | 12.70 | - | 9.53 | 17.48 | 12.70 | 12.70 | - | - | - | - | - | - | - | - |
| 34(850) | 863.60 | - | - | 7.92 | 12.70 | - | 9.53 | 17.48 | 12.70 | 12.70 | - | - | - | - | - | - | - | - |
| 36(900) | 914.40 | - | - | 7.92 | 12.70 | - | 9.53 | 19.05 | 12.70 | 12.70 | - | - | - | - | - | - | - | - |
| 40(1000) | 1016.00 | - | - | 9.53 | 14.3 | - | 9.53 | 26.20 | - | - | - | - | - | - | - | - | - | - |
Mis vahe on nominaalsete ja tolliste roostevabast terasest torudel?
Nominaalne suurus (DN):
Tavaliselt millimeetrites (mm) ekspresseeritakse nominaalne suurus toru ligikaudsele läbimõõdule või sisemise läbimõõdule.
See on nominaalne väärtus, mitte toru tegelik suurus. NäiteksDN50näitab, et nominaalne läbimõõt on umbes 50 mm, kuid tegelik välimine läbimõõt võib olla60,3mm, sõltuvalt seina paksusest.
Niminalseid suurusi kasutatakse laialdaselt rahvusvahelistes standardites, eriti Euroopas ja Aasias.
Tolli suurus (NP):
Tollides (tollides) ekspresseeritud tolli suurus viitab nominaalse toru suurusele (NPS).
Seda nimetamiskonventsiooni kasutatakse tavaliselt keiserlike süsteemide riikides nagu Ameerika Ühendriigid.
NäiteksNps 1Torul on tegelik välimine läbimõõt33,4mm, mitte 1 tolli (25,4 mm).