304 Stainless Steel Pipe for Potable Water Systems304 Stainless Steel Sheet for Architectural Decoration304L Stainless Steel Coil for Marine Equipment Parts

STANDARDNE UNS WNR. AFNOR ET JIS BS GOST
SS 304 S30400 1.4301 Z7CN18-09 X5CrNi18-10 SUS 304 304S31 08Х18Н10
SS 304L S30403 1.4306/1.4307 Z3CN18-10 X2CrNi18-9 / X2CrNi19-11 SUS 304L 304S11 03Х18Н11
SS 304H S30409 1.4301 - - - - -

Roostevabast terasest 304/304L/304H torude ja torude keemiline koostis

  C Mn Si P S Kr Ni N
304 0,07 max 2,0 max 0,75 max 0,045 max 0,03 max min: 18,0 max: 20,0 min: 8,0 max: 10,5 -
304L 0,03 max 2,0 max 0,75 max 0,045 max 0,03 max min: 18,0 max: 20,0 min: 8,0 max: 12,0 0,10 max
304H min: 18,0
max: 20,0
min: 8,0
max: 10,5
min: 0,04
max: 0,10
0.75
max
2.0
max
0.045
max
0.03
max
0.10
max

Roostevabast terasest 304/304L/304H torude ja torude mehaanilised omadused

Hinne Tõmbetugevus ksi (min) Saagistugevus 0,2% ksi (min) Pikendus % Kõvadus (Brinell) MAX Kõvadus (Rockwell B) MAX
304 75 30 40 201 92
304L 70 25 40 201 92
304H 75 30 40 201 92